This study aims to investigate the feasibility of recovering and utilizing powder coating waste within a Polyamide 6 (PA6) and to evaluate the effect of these particles on the properties of the resulting composite. Neat PA6 served as the reference, while formulations containing 5, 15, and 25 wt.% powder coating waste, combined with 1, 3, and 5 wt. % compatibilizer were prepared. Structural, thermal, and morphological analyses were conducted alongside evaluations of mechanical and physical properties. FTIR analysis confirmed the formation of covalent bonds between the maleic anhydride groups of the compatibilizer and the amine groups of the PA6 matrix. DSC and TGA results indicated that the optimal formulation (5 wt.% waste with 5 wt.% compatibilizer) enhanced thermal stability and acted as a nucleating agent within the PA6 crystalline structure. SEM images revealed a transition from the smooth fracture surface of neat PA6 to a fully continuous morphology in the optimal composite, free of interfacial voids. Adding waste in excess of 5 wt. % resulted in a deterioration of properties.
کلیدواژهها [English]